Never used Cerakote, but I used Duracoat and I obtained the same results as Mike45 posted. I was very unimpressed. If I were going to spend my money on something other than bluing, I would look into the ion-bond type treatments like Hard Hat.
__________________
Brown's Custom Grips
Exotic wood pistol grips for 1911 frames.
Find US On Facebook!

Class 07 FFL and Dan Wesson Dealer
Reply With Quote
  #2  
Old 12-07-2011, 06:12 AM
zenfly zenfly is offline
Founding Member
COTEP Member
 
Join Date: Aug 2011
Location: Cape Canaveral
Posts: 79
Thanks: 0
Thanked 2 Times in 2 Posts
Default

From all I've read in reports over the years there are two best choices..
Severns custom Hard Hat, or DLC IonBond is what they coat oil well drill bits for drilling through rock.. IonBond is also used on cutter bits for hard metals..
I've never read a report about anyone who wasn't thrilled with Hard Hat or any of Severns work and will be my choice when CBOB gets a little more beat up..
__________________
Drag not your strength from government but from the voices they abuse

COTEP #236
Reply With Quote
  #3  
Old 12-07-2011, 07:35 AM
titanse05's Avatar
titanse05 titanse05 is offline
Founding Member
COTEP Member
 
Join Date: Apr 2011
Location: Near Somerset, PA
Posts: 734
Thanks: 26
Thanked 31 Times in 7 Posts
Default

If you want a black coating, Hard Hat is the only way to go. My Fusion has the ion-bond treatment and I'm not all that impressed with it. The Duty Coat on my CCO is 100 times better than the ion-bond and I would imagine that the Hard Hat is at least as good as the duty coat.
__________________
CBOB0235
Reply With Quote
  #4  
Old 12-07-2011, 12:37 PM
zenfly zenfly is offline
Founding Member
COTEP Member
 
Join Date: Aug 2011
Location: Cape Canaveral
Posts: 79
Thanks: 0
Thanked 2 Times in 2 Posts
Default

Quote:
Originally Posted by titanse05 View Post
If you want a black coating, Hard Hat is the only way to go. My Fusion has the ion-bond treatment and I'm not all that impressed with it. The Duty Coat on my CCO is 100 times better than the ion-bond and I would imagine that the Hard Hat is at least as good as the duty coat.
So... there ya'go..Glad to hear that. It was the way I was going..
__________________
Drag not your strength from government but from the voices they abuse

COTEP #236
Reply With Quote
  #5  
Old 12-07-2011, 06:34 PM
SemperFi1977m's Avatar
SemperFi1977m SemperFi1977m is offline
Founding Member
COTEP Member
 
Join Date: Apr 2011
Location: Missouri
Posts: 442
Thanks: 5
Thanked 0 Times in 0 Posts
Default

And if youre a poor boy like me or just dont want to dump alot into a beater gun lol....
Freedom gunworks has a nitride bath treatment for 150. He calls it Atranite. I havent used it yet, but i will be giving it a try.
__________________
COTEP #0443 USMC #0311
"Do your duty in all things. You cannot do more, you should never wish to do less." ~Robert E Lee
“The hottest places in hell are reserved for those who in times of great moral crises maintain their neutrality.” ~Dante Alighieri
Reply With Quote
  #6  
Old 12-09-2011, 12:49 AM
m60g m60g is offline
Founding Member
COTEP Member
 
Join Date: Dec 2011
Location: Colorado
Posts: 23
Thanks: 0
Thanked 0 Times in 0 Posts
Default

I'm pretty set on IonBond, but Cerakote is right there in the running. I really like the choice of colors in Cerakote, I just don't think it is as tough as IonBond.


I've got a pm out to Dave Severns about his Hard Hat, not quite sure what this on is about yet